about the interface between two grains
Posted: Wed Jul 11, 2012 10:45 am
Dear Bernd:
I met a problem that when the two grains of the same phase (fcc_a1(al) grown in liquid phase) grow to contact each other, the interface seems not smooth, as shown in fig 1.
The domain is 200*200, dx=1micrometer. I have increased the interface energy of fcc_a1/fcc_a1 phase from 5E-6J/cm**2 to 1E-3 J/cm**2 or decrease it to no_phase_interaction. It seems the interface is still not good when the two grains of the same phase contact.
Thank you very much.
Best wishes.
swh
I met a problem that when the two grains of the same phase (fcc_a1(al) grown in liquid phase) grow to contact each other, the interface seems not smooth, as shown in fig 1.
The domain is 200*200, dx=1micrometer. I have increased the interface energy of fcc_a1/fcc_a1 phase from 5E-6J/cm**2 to 1E-3 J/cm**2 or decrease it to no_phase_interaction. It seems the interface is still not good when the two grains of the same phase contact.
Thank you very much.
Best wishes.
swh